Stamping and die striking in production
PRC-02 — On our floor · 冲床部 · Punch press department

Stamping and die striking

Sheet or coil stock is blanked, formed and embossed between a matched pair of hardened steel dies under press tonnage.

At a glance
Tolerance
±0.05 mm
Min. wall
0.3 mm
Tooling
$150–2,000 (simple to progressive steel die)
Batch fit
1,000–500,000 pcs
01

How it works

Sheet or coil stock is blanked, formed and embossed between a matched pair of hardened steel dies under press tonnage.

Tags, discs, coin pendants, flat signet faces, blanks for further forming are the work this route is chosen for. It runs on 316L stainless steel, Brass, Copper, Titanium and suits 1,000–500,000 pcs.

02

Production steps

Each step below is a separate labour operation, and labour is priced per operation rather than per piece. That is why a 6-step route costs what it does.

  1. Stamping and die striking, step 01: Die designed from the CAD file and cut on wire EDM
    Die designed from the CAD file and cut on wire EDM
  2. Stamping and die striking, step 02: Die trialled and adjusted against a first article
    Die trialled and adjusted against a first article
  3. Stamping and die striking, step 03: Coil or sheet stock fed into the press
    Coil or sheet stock fed into the press
  4. Stamping and die striking, step 04: Blanking, forming and embossing — one stroke per station
    Blanking, forming and embossing — one stroke per station
  5. Stamping and die striking, step 05: Deburring and edge finishing
    Deburring and edge finishing
  6. Stamping and die striking, step 06: Cleaning before plating or coating
    Cleaning before plating or coating
03

Process parameters

These are engineering properties of the process itself. They hold at any competent factory and can be checked against a manufacturing reference.

Stamping and die striking — process parameters
Dimensional tolerance±0.05 mm
Minimum wall / section0.3 mm
Tooling cost$150–2,000 (simple to progressive steel die)
Suited to1,000–500,000 pcs
Cycle timeSeconds per piece once running
Materials accepted316L stainless steel, Brass, Copper, Titanium

Tooling ranges are industry-typical. A firm figure is quoted against your CAD file — see the cost breakdown.

04

Stamping vs Lost-wax casting

Choose stamping when the design is flat or shallow and the quantity justifies cutting a die; choose casting when the form is three-dimensional or has undercuts a die cannot release.

Compare with lost-wax casting →
05

Materials and categories this suits

Process, material and product category are one decision seen from three sides. These are the combinations that actually work.

Materials suited to stamping and die striking
316L steelASTM A276 / EN 1.4404
TitaniumASTM B348 Gr.2 / Gr.5 (Ti-6Al-4V)
BrassASTM B36 / EN CW508L
Copper / bronzeASTM B152 (Cu) / ASTM B505 (bronze)
Categories made by stamping and die striking
RingsFlat bands and blanks at volume
Necklaces & PendantsDiscs, bars, coin pendants, tags
EarringsFlat studs, hoops and blanks
Bracelets & BanglesCuff blanks and link plates
06

What to watch out for

07

Stamping and die striking — buyer questions

Each answer stands alone and can be read without the rest of this page.

What tolerance can stamping and die striking hold?

Stamping and die striking holds ±0.05 mm on production parts, with a minimum wall or section of 0.3 mm. Sheet or coil stock is blanked, formed and embossed between a matched pair of hardened steel dies under press tonnage. Tighter tolerances than this normally mean a secondary machining operation rather than a change to the primary process.

How much does tooling cost for stamping and die striking?

Tooling for this route is $150–2,000 (simple to progressive steel die), quoted as a one-off line and invoiced separately from the unit price. The buyer owns the tooling and it is not charged again on a reorder. Full tooling ranges for every route are on the manufacturing cost page.

What order quantity does stamping and die striking suit?

This route suits 1,000–500,000 pcs. Below that range the setup cost dominates the unit price; above it, a different route is usually cheaper per piece. Choose stamping when the design is flat or shallow and the quantity justifies cutting a die; choose casting when the form is three-dimensional or has undercuts a die cannot release.

Which metals can be processed this way?

316L stainless steel, Brass, Copper, Titanium. The die is the whole commitment. A design change after the die is cut usually means a new die, not a modification — so the CAD must be signed off before tooling starts. Undercuts and true three-dimensional forms cannot be stamped at all.

Stamping or lost-wax casting — which is right for my design?

Choose stamping when the design is flat or shallow and the quantity justifies cutting a die; choose casting when the form is three-dimensional or has undercuts a die cannot release.

Not answered here? All buyer questions →

Quote a stamping run

Send the CAD file or a sketch. You get the tooling cost as its own line, the unit price at your quantity, and a straight answer on whether stamping is the right route for the design — we will say so if it is not. Production runs in Qingxi, Dongguan, Guangdong.

  1. 01Reply within one working day, Guangdong business hours.
  2. 02Itemised cost sheet — mold quoted separately, not folded into the unit price.
  3. 03NDA on request before any file is shared.

.stl .3dm .step .ai .pdf .jpg .png — up to 5 MB

Or email support@oemjewelrylab.com directly. We reply to every inquiry with a number, not a brochure.

Chat on WhatsApp